MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Guarniflon PTFE G800 Polytetrafluoroethylene
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded; Polytetrafluoroethylene (PTFE), Molded

Material Notes: A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric properties

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.14 - 2.18 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 24.0 MPaextruded; ASTM D4894
 >= 30.0 MPamolded; ASTM D4894
Elongation at Break >= 300 %extruded; ASTM D4894
 >= 400 %molded; ASTM D4894
Compressive Yield Strength 5.00 - 6.00 MPa
@Strain 1 %
ASTM D695
Coefficient of Friction, Dynamic 0.060ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 40.0 kV/mmin air, extruded; ASTM D149
 >= 60.0 kV/mmin air, molded; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Guarniflon PTFE G400 Polytetrafluoroethylene
Guarniflon PTFE G500 Polytetrafluoroethylene
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Overview of materials for Polytetrafluoroethylene (PTFE), Molded

PGUARN005 / 142738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.