Description: Vacuum bagging film. Ideally suited to aerospace and wind energy applications. Features & Benefits: - Tough, high elongation elastomeric film, suitable for de-bulking applications and oven curing of composites up to temperature of 150°C (302°F)
- Due to the film’s high elasticity, the necessity for pleats is reduced in debulk operations
- Premium film for wind energy applications
- Excellent recovery after elongation enables the film to be reused on subsequent debulk operations, making this film one of the most cost effective debulk products in our range
- Good release from sealant tape
Information provided by Cytec, subsequently acquired by Solvay. |