MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impact strength, oil and solvent resistance and creep resistance at elevated temperatures.

Typical applications include replacements for die castings and sheet molding compounds, valve covers, intake manifolds, oil pans and circuit breakers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.71 g/cc
Water Absorption 0.15 %24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 50 - 60
Tensile Strength, Ultimate 14000 - 17000 psi
Flexural Strength 30000 - 35000 psi
Compressive Strength 19000 - 24000 psi
Izod Impact, Notched 21.0 - 26.0 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 380 - 400 V/milShort Time
Arc Resistance >= 180 sec
Comparative Tracking Index >= 600 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °F
Flammability, UL94 HB
@Thickness 3.17 mm
 HB
@Thickness 1.59 mm
 V-0
@Thickness 6.35 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC
A. Schulman BMC 6241 Glass Fiber Reinforced Compound
A. Schulman BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 300 Mineral Filled, Glass Reinforced Polyester
A. Schulman BMC 5209 Mineral Filled, Glass Reinforced Polyester

PBMC027 / 27210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.