MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt HANDY HI-TEMP 548® Carbide Brazing Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes:

Applications: Handy Hi-Temp 548 is a modified nickel-silver filler metal primarily used to join tungsten carbide to steel. Brazing is often combined with heat treatment of the steel tool bits. The filler metal has good high temperature strength and toughness.

Characteristics:This filler metal exhibits excellent flow and wetting characteristics on tungsten carbides and tool steels, especially when induction brazed. The material also has good gap filling properties and plasticity at brazing temperature while being resistant to the joint cracking tendencies of the standard nickel-silver materials. For induction, torch or furnace brazing use Handy Hi-Temp M Flux or Handy Hi-Temp Boron Modified Flux.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.302 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 28000 - 30000 psiTungsten Carbide/ SAE 8740 Steel lap joint.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000263 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 1615 - 1685 °F
Solidus 1615 °FMelting Point
Liquidus 1685 °FFlow Point
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1700 - 1900 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 54 - 56 %
Manganese, Mn 3.5 - 4.5 %
Nickel, Ni 5.5 - 6.5 %
Other, total <= 0.50 %
Silicon, Si 0.010 - 0.40 %
Zinc, Zn >= 32.1 %
 
Descriptive Properties
ColorLight Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8640 Steel, quenched 845°C (1550°F), 650°C (1200°F) temper
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene
AISI 8640 Steel, quenched 845°C (1550°F), 540°C (1000°F) temper
AISI 8640 Steel, quenched 845°C (1550°F), 425°C (800°F) temper

NLUCMI09 / 18076

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.