MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Wire & Cable W2402 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8615 sec; ASTM D2240
Tensile Strength at Break 19.0 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 360 %Type IV, 510 mm/min; ASTM D638
Tensile Modulus 8.69 MPaType IV, 510 mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 37.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °CUL Temperature Rating
Brittleness Temperature -46.0 °CASTM D746
Oxygen Index 26 %
@Thickness 1.91 mm
ASTM D2863
 
Descriptive Properties
AdditiveLead Stabilizer
FeaturesFlame Retardant
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Tensile Elongation90%121°C, 1.91 mm; 168 hr, UL Standard
UsesCable Jacketing
 Communication Wire Jacketing
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable W2402L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable W9400L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable W2301 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable JLC31A Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable JKC30A Polyvinyl Chloride, Flexible

PH0POL0213 / 144782

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.