MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay Chemicals SOLID CAUSTIC SODA MICROPEARLS
Categories: Ceramic

Material Notes: Some applications of this product may be regulated or restricted by national or international standards (e.g. for food additives, water treatment, the pharmaceutical industry, etc). The buyer and the eventual user must independently determine the suitability of this product for any particular purpose and its manner of use.

EINECS Number: 215-185-5/CAS Number: 1310-73-2

Information provided by Solvay

Key Words: Sodium Hydroxide, NaOH
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 10 Mesh10 MeshOpening 2000µm; ASTM E11
 12 Mesh12 MeshOpening 1700µm; ASTM E11
 14 Mesh14 MeshOpening 1700µm; ASTM E11
 16 Mesh16 MeshOpening 1700µm; ASTM E11
 18 Mesh18 MeshOpening 1700µm; ASTM E11
 20 Mesh20 MeshOpening 1700µm; ASTM E11
 25 Mesh25 MeshOpening 1700µm; ASTM E11
 30 Mesh30 MeshOpening 1700µm; ASTM E11
 35 Mesh35 MeshOpening 1700µm; ASTM E11
 40 Mesh40 MeshOpening 1700µm; ASTM E11
 45 Mesh45 MeshOpening 1700µm; ASTM E11
 50 Mesh50 MeshOpening 1700µm; ASTM E11
 60 Mesh60 MeshOpening 1700µm; ASTM E11
 70 Mesh70 MeshOpening 1700µm; ASTM E11
 80 Mesh80 MeshOpening 1700µm; ASTM E11
 100 Mesh100 MeshOpening 1700µm; ASTM E11
 120 Mesh120 MeshOpening 1700µm; ASTM E11
 140 Mesh140 MeshOpening 1700µm; ASTM E11
 170 Mesh170 MeshOpening 1700µm; ASTM E11
 200 Mesh200 MeshOpening 1700µm; ASTM E11
 230 Mesh230 MeshOpening 1700µm; ASTM E11
 270 Mesh270 MeshOpening 1700µm; ASTM E11
 325 Mesh325 MeshOpening 1700µm; ASTM E11
 400 Mesh400 MeshOpening 1700µm; ASTM E11
Molecular Weight 40.01 g/mol40.01 g/mol
 
Descriptive Properties
ColorWhite
Composition<0.1 mg/kgHg, ISO 5993
 <0.5 mg/kgPb
 <1 mg/kgCd
 <1 mg/kgCr
 <10 mg/kgFe, ISO 6685
 <2 mg/kgNi, ISO 11885
 <2 mg/kgAs
 <200 mg/kgNaCl, ASTM E1787
 <4 g/kgNa2CO3, ISO 3196
 <5 mg/kgSb
 <5 mg/kgSe
 <80 mg/kgNa2SO4, ASTM E1787
 >990 g/kgNaOH, ISO 979

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Chemicals Liquid Caustic Soda (Sodium Hydroxide, NaOH) 90-99% Aqueous Solution
Formosa Plastics 50% Liquid Caustic Soda Membrane Grade

WSOLV126 / 147775

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.