MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos CAP311US2 High Density Polyethylene copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: CAP311US2 is a High Density Polyethylene copolymer manufactured by INEOS Olefins & Polymers intended for the injection and compression molding of screw caps for still mineral water and lightly pressurized beverages. Developed for applications requiring excellent process ability, high rigidity, enhanced stress cracking resistance and excellent organoleptic properties, CAP 311US2 is well suited for packaging in direct contact with beverages and sensitive food. CAP311US2 contains a slip package for lower cap removal torques and improved capping performance. This material meets the Food and Drug Administration requirements of 21 CFR 177.1520.

Information provided by INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D4883
ESCR 100% Igepal® 62 hour62 hourCondition B, 100% Igepal, F50; ASTM D1693
ESCR 10% Igepal® 21 hour21 hourCondition B, F50; ASTM D1693
Melt Flow 3.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 28.8 MPa4180 psi2 in/min; ASTM D638
Elongation at Break >= 900 %>= 900 %2 in/min; ASTM D638
Flexural Modulus 1.55 GPa225 ksiTangent; ASTM D790
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²ASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21CFR 177.1520
 
Descriptive Properties
Molecular Weight DistributionBimodalINEOS Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOS857 / 291463

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.