System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Sirmax Dafnemid® 66XA P05/T Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, Glass Fiber Filled, Flame Retardant
Material Notes:
25% glass fibers. RTI ratings up to 140°C at 0.8 mm thickness. Heat stabilized. Flame Retardant grade With halogens.
Application: Injection Molding
Information provided by Sirmax®
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.50
-
1.55
g/cc
ISO 1183
Linear Mold Shrinkage
0.0020
-
0.0050
cm/cm
Mechanical Properties
Original Value
Comments
Hardness, Rockwell L
100
ISO 2039-2
Tensile Strength at Break
120
MPa
50 mm/min; ISO 527-2
Elongation at Break
4.5 %
50 mm/min; ISO 527-2
Tensile Modulus
10000
MPa
1 mm/min; ISO 527-2
Flexural Strength
200
MPa
2 mm/min; ISO 178
Flexural Modulus
8500
MPa
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
9.00
kJ/m²
ISO 180/1A
Charpy Impact Unnotched
50.0
kJ/m²
ISO 179/1eU
Charpy Impact, Notched
9.00
kJ/m²
ISO 179/1eA
Electrical Properties
Original Value
Comments
Comparative Tracking Index
400
V
IEC 60112
Thermal Properties
Original Value
Comments
Hot Ball Pressure Test
165
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
250
°C
ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
ISO 75/Af
Vicat Softening Point
230
°C
B50; ISO 306
245
°C
A50; ISO 306
Flammability, UL94
V-0
@Thickness 0.800 mm
V-0
@Thickness 3.00 mm
Glow Wire Ignition Temperature
875
°C
@Thickness 1.00 mm
IEC 60695-2-13
930
°C
@Thickness 1.50 mm
IEC 60695-2-13
930
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Melt Temperature
280
-
300
°C
ISO 294
Mold Temperature
90.0
°C
ISO 294
Drying Temperature
80.0
-
100
°C
Dry Time
3.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSIRMX045 / 281148
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.