MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite GF 8202 L12 Phenolic Novolac Molding Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: GF 8202 L12 is a fiberglass reinforced modified phenolic novolac molding compound, with 12 mm chop length. This compound features superior strength properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Apparent Bulk Density 0.300 g/ccASTM D1895
Water Absorption 0.050 %
@Time 86400 sec
ASTM D570
 0.20 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage <= 0.0010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 105ASTM D785
Hardness, Rockwell M 120ASTM D785
Tensile Strength 120 MPaASTM D638
Flexural Strength 260 MPaASTM D790
Flexural Modulus 22.0 GPaASTM D790
Compressive Strength 320 MPaASTM D695
Izod Impact, Notched 900 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 10.0 kV/mm
@Frequency 60 Hz
SS; ASTM D149
 >= 12.0 kV/mm
@Frequency 60 Hz
ST; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 282 °CPost Baked; ASTM D648A
Shrinkage <= 0.10 %Post; ASTM D955

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite GF 8202 L24 Phenolic Novolac Molding Compound
Westlake Plastics Zelux® GS Polycarbonate - Gamma Stabilized For Medical Applications
Norplex-Micarta NP193PM Phenolic Laminate Sheet
Celanese Zytel® 80G33HS1L NC010 PA66-IGF33
A. Schulman BMC T44-15613 High Strength Mineral Filled Molding Compound

PSUMIT188 / 193993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.