MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Description

Formion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.
Application

Formion® FI 120E is targeted for exterior or interior appearance or packaging applications in film, blow molding, thermoforming or extrusion applications, which may require high or low gloss, excellent colorability or transparency.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccISO 1183/1
Linear Mold Shrinkage 0.0060 - 0.018 cm/cm
@Thickness 3.20 mm,
Time 259000 sec
ISO 294
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6315 sec delay; ISO 868
Tensile Strength, Ultimate 21.0 MPaat max load; ISO 527
Elongation at Break 225 %ISO 527
Flexural Modulus 0.227 GPaTangent; ISO 178
Izod Impact, Notched (ISO) NBISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °C10°C per minute; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 39.0 °C
@Thickness 3.17 mm
ISO 75
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
E-Polymers EFLEX® I2020 Ionomer
ExxonMobil Iotek® 7510 Zinc Ionomer Molding/Extrusion Resin
Overview of materials for Ionomer, Film Grade
A. Schulman FORMION™ FI 243 Ionomer
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin

PASHU021 / 24985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.