MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SIMONA America SIMONA® 010023689 PVC CRP-1 FM 4910
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Fire-safe PVC material formulated for outstanding fire retardancy, FM 4910 listed

Information provided by Simona America Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.415 g/cc1.415 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %ASTM D570
Thickness 6350 microns250 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484ASTM D2240
Tensile Strength, Yield 51.7 MPa7500 psiASTM D638
Flexural Modulus 3.34 GPa485 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 57.6 µm/m-°C32.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 72.2 °C162 °F
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C162 °FASTM D648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colorwhite
Length (in)120
Regulatory CodeFM 4910
Width (in)48

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIMONA371 / 285099

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.