MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SMAC CABLE® 25235-20-08 Damping Material
Categories: Other Engineering Material

Material Notes: The SMAC CABLE® wire rope isolators are entirely metallic and possess multi-axis characteristics. They are well adapted for the isolation of materials exposed to shock and vibration in harsh environment.

Descriptions
Bars: Aluminum alloy
Screws: Inox A2
Threaded insert: Stainless steel
Standard treatment: SurTec 650

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 180 - 300 °C356 - 572 °F
 
Descriptive Properties
Damping Factor0.1 - 0.2
F, Max Dynamic1020 daN50.0 mm, 45° down and out
 2125 daN51.0 mm, down
 2875 daN20.5 mm, up
 550.0 daN21.7 mm, up and down
 835.0 daN30.0 mm, left and right
F, Max Static250.0 daN8.0 mm, up and down
 250.0 daN9.3 mm, left and right
 400.0 daN10.0 mm, 45° down and out
 500.0 daN7.5 mm, down
 500.0 daN4.5 mm, up
Transmissibility at resonance3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZSMAC075 / 146191

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.