MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Uniplex DOS Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex DOS is a low-temperature and light-resistant plasticizer for PVC, PS, cellulosics and rubber. In PVC Uniplex DOS exhibits an advantageous blend of properties such as an excellent low temperature flexibility combined with a low volatility.

Chemical composition: Di-(2-Ethylhexyl) Sebacate

CAS reg. no.: 122-62-3

General Uniplex DOS has

  • a low viscosity, which, in combination with its weak ability to solvate PVC, has a positive effect on the initial viscosity and storage stability of plastisols.
  • a lower volatility compared to the corresponding adipate.
Uniplex DOS imparts
  • a very good low-temperature resistance to suitably plasticized compounds; this effect is clearly noticeable even when Uniplex DOS is used in combination with other plasticizers.
  • very good light stability to PVC compound.
Applications: Uniplex DOS is used for a wide range of articles based on polyvinyl chloride (PVC), polystyrene (PS), cellulosics (cellulose acetate), and rubber (chloroprene, nitrile, butadiene). It is particularly beneficial to use Uniplex DOS when very good low-temperature flexibility and light stability are required, together with a low volatility.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.913 g/cc
Viscosity 24 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.10[mg KOH/g]
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Karl Fischer
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear liquid
Assay>99%
Color<50Hazen
Specifications164°CDissolution temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9117 / 209508

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.