MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical Propylene
Categories: Fluid

Material Notes: Physical Properties: Highly reactive in polymerization and addition reaction. and Colorless, Narcotic gas

Structure & Characteristics: Structure and characteristics: CH2=CH-CH3. A colorless inflammable liquefied gas which has characteristic odor of hydrocarbon

Uses: Film, Plastic, Product, PP resin, Urethane resin, Surfactant, Allyl alcohol, Glycerin epoxy resin, Agricultural medicine, Antioxidant, Plastics, Acetone, Solvent, Paint, Glycerin, Epoxy resin

CAS: 115-07-1

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.510 g/cc
Vapor Pressure 7060 torr
@Temperature 20.0 °C
Vapor Density=1.48
 
Thermal PropertiesOriginal ValueComments
Boiling Point -48.0 °C
Flash Point -108 °C
Ignition Temperature 455 °CAutoignition
 
Descriptive Properties
ComponentsBUTENE + BD + CYCLOPROPANE + BUTANE<5 ppm
 C2 & LIGHTER<100 ppm
 CO<5 ppm
 CO2<5 ppm
 H2O<5 ppm
 MA & PD<5 ppm
 METHANO<10 ppm
 O2<5 ppm
 PROPANE<0.4%
 PROPYLENE>99.9%
 SULFUR<2 ppm, as H2S

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexane (C6H14)
Acetylene, Ethyne, C2H2
2-Methylbutane, C5H12
n-Heptane, C7H16
Butane (C4H10)

PLAY766 / 148776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.