MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shin-Etsu Silicones LIMS™ KE2001-40A/B Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Information Provided by Shin-Etsu Silicones of America, Inc.

Key Words: LSR, Liquid Silicone Rubber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Viscosity 400000 cPA
 400000 cPB
Linear Mold Shrinkage 0.022 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
Tensile Strength 9.20 MPa
Elongation at Yield 600 %
100% Modulus 0.158 ksi
@Strain 100 %
Tear Strength 42.0 kN/m
Compression Set 5.0 %
@Temperature 200 °C,
Time 14400 sec
 40 %
@Temperature 150 °C,
Time 3600 sec
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 120 °C
Press Cure
 60.0 min
@Temperature 150 °C
Post Cure
 
Descriptive Properties
AppearanceTranslucent
Cure Rate20T10 (302°F, ODR)
 29T90 (302°F, ODR)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones LIMS™ KE2090-40AB Elastomer
Shin-Etsu Silicones LIMS™ KEG2001-40A/B Elastomer
Shin-Etsu Silicones KE-2090-20A/B Self-adhesive LIMS Silicone
Overview of materials for Polypropylene, Molded
Overview of materials for Polypropylene, Extrusion Grade

PSHIN014 / 103841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.