MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon R37908R015L Silicone Rubber/Fiberglass/Acrylic/Polyester
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Laminated film: aluminized PEN; Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2, layer 1: acrylic PSA; Side 2, layer 2: polyester substrate; Side 2, layer 3: acrylic PSA; Interleave: Release substrate

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 1.00 millaminated film; Arlon SQA-TMS-003
 1.00 milside 2 layer 2; Arlon SQA-TMS-003
 1.25 milside 2 layer 3; Arlon SQA-TMS-003
 1.25 milside 2 layer 1; Arlon SQA-TMS-003
 2.50 milside 1; Arlon SQA-TMS-003
 8.00 milsubstrate; Arlon SQA-TMS-003
 15.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 44silicone property; ASTM D2240
Tensile Strength, Ultimate 1100 psisilicone property; ASTM D412
Elongation at Break 650 %silicone property; ASTM D412
Adhesive Bond Strength 1.50 psiadhesion to Al initially; Arlon SQA-TMS-011
 2.50 psiadhesion to Al at 24 hours; Arlon SQA-TMS-011
 4.00 psiadhesion to Al at 72 hours; Arlon SQA-TMS-011
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 320 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 23.9 °C
 
Descriptive Properties
ColorSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Corporation RO4450F Prepreg
A. Schulman ComAlloy® E-12672 Polyester Alloy
Mid-Mountain Materials HYTEX® 2200 Ceramic Fiber Industrial Textile
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches
Corning Pyroceram® Code 9606 Glass Ceramic

PARL065 / 79717

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.