MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 800 SI 2 HB Acetal (POM), Silicone Lubricated - UL94 HB
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Silicone Filled

Material Notes: RTP 800 SI 2 HB is a silicone fluid lubricated acetal. It offers easy flow, an excellent molded surface and good wear resistance.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D 792
Water Absorption 0.22 %
@Time 86400 sec
ASTM D 570
Additive Loading 2.0 %Primary Additive
Linear Mold Shrinkage 0.025 - 0.035 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 360 ksiASTM D 638
Flexural Strength 10300 psiASTM D 790
Flexural Modulus 330 ksiASTM D 790
Izod Impact, Notched 1.80 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D 257
Dielectric Strength 500 V/milShort Term; In Oil; ASTM D 149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 305 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 230 °FASTM D 648
Flammability, UL94 HB
@Thickness 0.800 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 425 °F
Mold Temperature 175 - 225 °F
Drying Temperature 250 °F
@Time 7200 sec
Moisture Content 0.15 %
Dew Point -25.0 °F
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupital® LO-21A Copolymer Acetal
RTP Company RTP 899 X 93924 Acetal (POM); Wear Resistant - Perfluoropolyether Oil - PTFE Lubricated
RTP Company RTP 800 TFE 5 HB Acetal (POM), PTFE Lubricated - UL94 HB
Overview of materials for Acetal Copolymer, Silicone Filled
Mitsubishi Iupital® WA-11H Copolymer Acetal

PQZWA2252 / 91048

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.