MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott FG13 Conversion Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..

Similar glasses include BG34, FG3

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.78 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 3.4
Alkali Class, AR 1
Stain Resistance Class, FR 1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.60 µm/m-°C
@Temperature -30.0 - 70.0 °C
 10.5 µm/m-°C
@Temperature 20.0 - 300 °C
Transformation Temperature, Tg 566 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55
@Wavelength 706.5 nm
He
 1.56
@Wavelength 587.6 nm
He
Transmission, Visible <= 2.0 %
@Wavelength 400 - 460 nm
 78 %
@Wavelength 700 nm
Internal transmittance of 86% at 700 nm.
IR Transmittance 87 - 88 %
@Wavelength 1500 - 2100 nm
Internal transmittance of 96-97% from 1500-2100 nm.
UV Transmittance <= 0.0010 %
@Wavelength 200 - 390 nm
Internal transmittance of 0.001% from 200-390 nm.
Reflection Coefficient, Visible (0-1) 0.91
@Wavelength 587.6 nm
Reflection Factor P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSGT67 / 2056

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.