MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® A-700 with 2.5 phr Curative, 3 phr Ca(OH)2, and 6 phr Maglite® D
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Viton® A-700 is an “A-family” gum polymer that has demonstrated easy processing. This gum provides:
  • Improved compression set resistance
  • Good flow for compression molding
  • Good mold release
  • Less mold fouling
  • Improved compression set resistance
  • Improved tear properties

Applications:

  • Compression molding of O-rings, gaskets, and other sealing devices
  • Extruded cords, profiles and tubing, or calendered sheets, when a blend of gum polymers are used
  • Blending with other polymers for viscosity modification

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7272Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D2240-91
Tensile Strength, Ultimate 13.8 MPa2000 psiCured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
Elongation at Break 215 %215 %Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
100% Modulus 6.10 MPa
@Strain 100 %
885 psi
@Strain 100 %
Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412-92
Tear Strength 24.0 kN/m137 pliDie C, Cured 10 min at 177°C and Post Cured 24 hr at 232°C
Compression Set 13 %
@Temperature 200 °C
13 %
@Temperature 392 °F
Method B, O-rings 70 hr; ASTM D1414-94
 
Descriptive Properties
Formulation as Tested2.5Viton® Curative No. 50
 3Calcium Hydroxide
 30MT Black (N-990)
 6Maglite® D
 97.5Viton® A-700

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDVD73 / 33943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.