MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Trinseo EMERGE™ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: EMERGE™ PC/ABS 7570 advanced resin is a high flow, ignition-resistant PC/ABS blend that contains no chlorinated for brominated additives. Its superior processing makes it ideal for injection molding of large, thin-wall, or intricate parts. EMERGE™ PC/ABS 7570 is suitable for use in a wide variety of applications in the Information Technology Equipment & Consumer Electronics industries.

Applications:

  • LCD TV Enclosures
  • CRT TV Enclosures
  • Monitor and PC Enclosures

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183/B
Apparent Bulk Density 0.670 g/cc0.0242 lb/in³ISO 60
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow  20 g/10 min
@Load 3.80 kg,
Temperature 230 °C
20 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 95 g/10 min
@Load 5.00 kg,
Temperature 260 °C
95 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.0 MPa
@Thickness 4.00 mm
6820 psi
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Tensile Strength, Yield 60.0 MPa
@Thickness 4.00 mm
8700 psi
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Elongation at Break 40 %
@Thickness 4.00 mm
40 %
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Elongation at Yield 4.0 %
@Thickness 4.00 mm
4.0 %
@Thickness 0.157 in
Injection Molded; ISO 527-2/50
Tensile Modulus 2.60 GPa
@Thickness 4.00 mm
377 ksi
@Thickness 0.157 in
Injection Molded; ISO 527-2/1
Flexural Strength 92.0 MPa
@Thickness 4.00 mm
13300 psi
@Thickness 0.157 in
Injection Molded, 2.0 mm/min; ISO 178
Flexural Modulus 2.70 GPa392 ksiInjection Molded, 2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²ISO 180/A
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 95.0 °C203 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FUnannealed; ISO 75-2/A
Vicat Softening Point 98.0 °C208 °FISO 306/B50
 105 °C221 °FISO 306/A120
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
All Colors
 V-0
@Thickness 2.50 mm
V-0
@Thickness 0.0984 in
Natural plus Color
Glow Wire Ignition Temperature 800 °C
@Thickness 2.00 mm
1470 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical AF342F ABS, Flame Retardant, High Flow
Mitsubishi Xantar® C CF 407 Polycarbonate/ABS Blend
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Trinseo EMERGE™ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Covestro Bayblend® FR3000 PC/ABS Blend

PDWST058 / 142267

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.