MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Silberline Aquavex™ 1752-207S
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Aquavex™ grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary non-ionic surfactant/inhibitor carrier. Aquavex™ can be dispersed water or in a water/co-solvent blend. The inhibitor is effective at reducing the aluminum-water reaction in a broad range of waterborne ink resins. The surfactant/inhibitor system is compatible with many UV ink vehicles and the inhibitor provides stability for one pack UV ink formulations. The specific degree of stability is formulation dependent and each formulation must be evaluated for acceptable stability. High or excessive shear during processing will reduce the effectiveness of the inhibitor and should be avoided.

Applications: Printing Inks; Waterborne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 1.5 %1.5 %
Particle Size 21 µm21 µm
 
Descriptive Properties
% Carrier20
Aluminum Flake, wt%80
CategoryLeafing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ESIBER261 / 6016

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.