Characterization: Makrofol LM 322 2-4 160006 is an extruded polycarbonate film. Properties / Applications: Makrofol LM 322 2-4 160006 is an extruded polycarbonate film filled with light-scattering agent. It displays a smooth homogenous illumination of the front side of a backlight part even if a point source is applied. Typical applications are automotive instrument panels and backlight displays. Makrofol LM 322 2-4 160006 is available in a standard thickness of 0.012" (300 microns). Other thicknesses available on request. The surface structure of Makrofol LM 322 2-4 160006 is one side very fine matte, and one side fine matte. As with any product, use of Makrofol LM 322 2-4 160006 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |