MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC VALOX™ EH7020 PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: MINERAL FILLED, METALLIZABLE

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
Linear Mold Shrinkage, Flow  0.014 - 0.016 cm/cm
@Thickness 1.50 - 3.20 mm
0.014 - 0.016 in/in
@Thickness 0.0591 - 0.126 in
SABIC method
 0.015 - 0.016 cm/cm
@Thickness 3.20 - 4.60 mm
0.015 - 0.016 in/in
@Thickness 0.126 - 0.181 in
SABIC method
Linear Mold Shrinkage, Transverse  0.013 - 0.014 cm/cm
@Thickness 1.50 - 3.20 mm
0.013 - 0.014 in/in
@Thickness 0.0591 - 0.126 in
SABIC method
 0.014 - 0.015 cm/cm
@Thickness 3.20 - 4.60 mm
0.014 - 0.015 in/in
@Thickness 0.126 - 0.181 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 57.0 MPa8270 psi5 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 4.13 GPa599 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256
Izod Impact, Unnotched 3.89 J/cm7.29 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
ASTM D150
 3.1
@Frequency 50.0 - 60.0 Hz
3.1
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.9 kV/mm
@Thickness 3.20 mm
429 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.0039
@Frequency 50.0 - 60.0 Hz
0.0039
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 55.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
31.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 187 °C
@Thickness 6.40 mm
369 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 6.40 mm
221 °F
@Thickness 0.252 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 260 °C473 - 500 °FInjection Molding
Zone 1 240 - 255 °C464 - 491 °F
Zone 2 245 - 260 °C473 - 500 °F
Zone 3 250 - 265 °C482 - 509 °F
Melt Temperature 250 - 265 °C482 - 509 °F
Mold Temperature 65.0 - 90.0 °C149 - 194 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 12.0 hour12.0 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00250 - 0.00380 cm0.000984 - 0.00150 in
Screw Speed 50 - 80 rpm50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10267 / 243734

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.