MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper, UNS C43500
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability for forming and bending.

Applications: bourdon tubing and musical instruments.

Available as flat products and tube.

Key Words: ISO CuZn19Sn, CEN CW701R, 205 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.66 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 317 - 552 MPa
Tensile Strength, Yield 110 - 469 MPaDepending on temper
Elongation at Break 46 %in 177.8 mm.
Modulus of Elasticity 110 GPa
 110 GPa
Poissons Ratio 0.38calculated
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
 30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa
 40.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.4 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.380 J/g-°C
Melting Point 965 - 1005 °C
Solidus 965 °C
Liquidus 1005 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 79 - 83 %
Iron, Fe <= 0.050 %
Lead, Pb <= 0.10 %
Other, total <= 0.15 %
Tin, Sn 0.60 - 1.2 %
Zinc, Zn 18.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Copper, UNS C43000
8% Aluminum Bronze, UNS C61000
Copper, UNS C12000
Copper, UNS C40800

MC43500b1 / 11355

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.