MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impellers, fans, valves and pipe elbows.

Product Features:

  • Designed for application by stiff brush or squeegee
  • Provides outstanding resistance to impingement, entrainment and erosion/corrosion.
  • Primarily designed for resurfacing metal components used in fluid flow environments.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Thickness 254 microns10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 62.1 MPa9000 psi
Compressive Strength 89.6 MPa13000 psi
Shear Strength 19.3 - 19.48 MPa2800 - 2825 psiTensile Shear Adhesion
Abrasion 0.0800.080[g] per 1000 cycles, 1 kg, CS17 Wheel
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourInitial Set
 300 min5.00 hourFull Mechanical
 360 min6.00 hourMachining Time
 
Descriptive Properties
AppearanceGray, Blue, Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35295 / 170042

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.