MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling GLASGUARD 1130 Corrosion-Resistant Panels
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corrosion resistance, weatherability, and dielectric properties. This material meets NEMA criteria for grade GPO-3. Grade 1130 was developed to meet the requirements of the NYC Transit Authority. It has been pultruded into channel shaped covers for the electrified third rail and molded into flat panels for both a sign material and switchgear components.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.10 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 14600 psiLengthwise; ASTM D-638
 16000 psiCrosswise; ASTM D-638
Tensile Modulus 1.49e+6 psiLengthwise/Crosswise; ASTM D-638
Flexural Strength 20400 psiLengthwise; ASTM D-790
 23300 psiCrosswise; ASTM D-790
Flexural Modulus 1.39e+6 psiCrosswise; ASTM D-790
 1.41e+6 psiLengthwise; ASTM D-790
Adhesive Bond Strength 6100 psilbs.; NEMA 11.11
Izod Impact, Notched 11.3 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 12.4 kV/mmPerpendicular S/T in Air; ASTM D-149
Arc Resistance 192 secASTM D-495
Track Resistance 52200 secInclined Plane; ASTM D-2303
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
Flame Spread Index 12Radiant Panel; ASTM E-162
 20UL Standard 723; ASTM E-84
 
Descriptive Properties
Electric Strength kV, ASTM D14975Parallel, Condition A
 79Parallel, Condition D (48/50)
Smoke Developed115ASTM E-84
Standard ColorGray
UL Recognition File NumberR9599
UL Standard 723 Fuel Contributed0ASTM E-84

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC
IDI Composites C-210 Thermoset Polyester, Sheet
IDI Composites C-206 Thermoset Polyester, Sheet

PGLASX1 / 41945

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.