Product Description: Dresinate™ 91 rosin soap is a fluid, high solids, aqueous solution of potassium soap of tall oil rosin. It is designed primarily for applications that require soap solutions of as low a water content as practical and of viscosity low enough that it is possible to pump the soap at practical temperatures. It is used as an emulsifier ingredient in solvent cleaners and soluble oils for metal cleaning. Dresinate™ 91 provides highly stable emulsions over a wide range of water hardness when used in combination with petroleum sulfonates in soluble oil formulations. Application/Uses: - Building and Construction
- Emulsifiers
- Hot Melt Adhesives
- Lubricants
- Paint and Coatings
- Solventborne Adhesives
Key Attributes:- Dilutible with water and aqueous solutions of alcohols and glycols
- Provides highly stable emulsions
Information provided by Eastman |