MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Bioline Cored wire
Categories: Metal; Nonferrous Metal

Material Notes: Sandvik Bioline cored wire (SBCW) is a composite wire consisting of a Sandvik Bioline F562 CoCrMo alloy shell and a secondary alloy as the core material. The core material is typically pure silver (Ag) to promote increased conductivity relative to solid Sandvik Bioline F562. However, other core materials such as platinum (Pt), gold (Au) and tantalum (Ta) can be selected in order to increase the radiopacity or provide other unique combinations of properties to the composite wire. The standard core dimension is 25% by area, however other core sizes can be considered. The outer component is characterized by:
  • Excellent corrosion resistance
  • Excellent fatigue properties
  • High strength combined with good ductility
The inner silver core provides:
  • High electrical efficiency
  • Electrical conductivity
  • Low electrical resistance.
Sandvik Bioline cored wire can be used for cochlear implants, pacemaker, defibrillator leads and varicose vein surgery devices.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 800 MPa0% CW, 45 Silver CSA
 870 MPa0% CW, 40 Silver CSA
 940 MPa0% CW, 35 Silver CSA
 1010 MPa0% CW, 30 Silver CSA
 1055 MPa20% CW, 45 Silver CSA
 1080 MPa0% CW, 25 Silver CSA
 1130 MPa30% CW, 45 Silver CSA
 1130 MPa20% CW, 40 Silver CSA
 1185 MPa40% CW, 45 Silver CSA
 1205 MPa30% CW, 40 Silver CSA
 1215 MPa20% CW, 35 Silver CSA
 1225 MPa50% CW, 45 Silver CSA
 1260 MPa60% CW, 45 Silver CSA
 1275 MPa40% CW, 40 Silver CSA
 1300 MPa30% CW, 35 Silver CSA
 1320 MPa20% CW, 30 Silver CSA
 1335 MPa50% CW, 40 Silver CSA
 1380 MPa40% CW, 35 Silver CSA
 1380 MPa20% CW, 25 Silver CSA
 1385 MPa60% CW, 40 Silver CSA
 1405 MPa30% CW, 30 Silver CSA
 1450 MPa50% CW, 35 Silver CSA
 1485 MPa40% CW, 30 Silver CSA
 1495 MPa30% CW, 25 Silver CSA
 1500 MPa60% CW, 35 Silver CSA
 1560 MPa50% CW, 30 Silver CSA
 1570 MPa40% CW, 25 Silver CSA
 1615 MPa60% CW, 30 Silver CSA
 1635 MPa50% CW, 25 Silver CSA
 1695 MPa60% CW, 25 Silver CSA
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 0.015 %
Carbon, C <= 0.025 %
Chromium, Cr 19 - 21 %
Cobalt, Co 29.13 - 36.7 %
Iron, Fe 1.0 %
Manganese, Mn 0.15 %
Molybdenum, Mo 9.0 - 10.5 %
Nickel, Ni 33 - 37 %
Phosphorus, P <= 0.015 %
Silicon, Si 0.15 %
Sulfur, S <= 0.010 %
Titanium, Ti 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Bioline F1537 Cobalt Alloy Bar
AISI Type S15500 (15Cr-5Ni) Precipitation Hardening Stainless Steel transverse direction, condition H925
Materion Vit 1b Zirconium-Based Bulk Metallic Glass (BMG)
316 Stainless Steel, annealed wire, 13 mm diam.
Cabot 10 Tantalum Alloy (UNS R05255)

NSANDV5198 / 199762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.