MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company ESD C 100 HI Polypropylene (PP); Electrically Conductive - ESD Protection - Impact Modified
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D 792
Linear Mold Shrinkage 0.012 - 0.017 cm/cm
@Thickness 3.20 mm
ASTM D 955
Melt Flow 4.0 - 6.0 g/10 min
@Load 2.16 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2600 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 120 ksiASTM D 638
Flexural Strength 3500 psiASTM D 790
Flexural Modulus 130 ksiASTM D 790
Izod Impact, Notched 15.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1000 ohm-cmASTM D 257
Surface Resistance <= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 0.50 secFTMS101C; 4046.1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
Flame Spread <= 4.00 in/min
@Thickness 1.60 mm
Automotive; FMVSS 302
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 - 450 °F
Mold Temperature 90.0 - 150 °F
Drying Temperature 175 °F
@Time 7200 sec
Injection Pressure 10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 101 CC HI FR A Polypropylene (PP); High Impact - Glass Fiber - Chemically Coupled - Flame Retardant - Preliminary Datasheet
RTP Company ESD C 100 MF Polypropylene (PP), ESD Protection - Electrically Conductive - Medium MFR
RTP Company ESD C 100 FR Polypropylene (PP); Flame Retardant - ESD Protection - Electrically Conductive
RTP Company ESD A 100 LF  Polypropylene (PP) Dissipative - Low Flow
RTP Company ESD A 100 HF Polypropylene (PP); ESD Protection - Static Dissipative

PQZRA36887 / 206073

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.