MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco 6015 Phenolic, Briquette, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.630 g/ccASTM D1895
Density 1.72 g/ccASTM D792
Water Absorption 0.078 %ASTM D570
Linear Mold Shrinkage 0.00090 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 94ASTM D785
Tensile Strength, Ultimate 101 MPaASTM D638
Elongation at Break 0.84 %ASTM D638
Tensile Modulus 15.3 GPaASTM D638
Flexural Strength 163 MPaASTM D790
Flexural Modulus 15.1 GPaASTM D790
Compressive Strength 215 MPaASTM D695
Poissons Ratio 0.31ASTM D638
Shear Modulus 5.84 GPaCalculated
Izod Impact, Notched 44.0 J/mASTM D256
Charpy Impact, Notched 0.450 J/cm²ASTM D256
Impact 206J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+12 ohm-cmASTM D247
Dielectric Constant 5.0ASTM D150
Dielectric Strength 11.5 kV/mmStep by Step; ASTM D149
 16.3 kV/mmShort Time; ASTM D149
Dissipation Factor 0.028ASTM D150
Arc Resistance 184 secASTM D495
Comparative Tracking Index 175 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µm/m-°C
@Temperature 40.0 - 130 °C
TMA; ASTM E831
Maximum Service Temperature, Air 236 °CHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 279 °CASTM D648
Flammability, UL94 V-1
@Thickness 3.10 mm
Shrinkage 0.056 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 6401 Phenolic, Briquette, Injection Molded
Plenco 6343 Phenolic, Granular, Transfer Molded
Plenco 6301 Phenolic, Granular, Injection Molded
Plenco 5488 Phenolic, Granular, Injection Molded
Plenco 5350 Phenolic, Granular, Compression Molded

PLEM07 / 50683

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.