Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength properties, along with excellent drawability, allow downgauging in bag applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Antiblock: No
- Slip: No
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications:- Bag in a Box
- Barrier Food Packaging
- Blown Film
- Food packaging
- Form Fill and Seal Packaging
- General Packaging
- Heavy Duty Bags
- Label Film
- Multilayer Packaging Film
- Overwrap Film
- Packaging Films
- Premium Trash Bags
- Produce Bags
- Shrink Film
- Stand Up Pouches
- Trash Bags
Information provided by ExxonMobil |