MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound LC00AEX1 Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LC00AEX1 compound is based on Polyetheretherketone (PEEK) resin containing 50% carbon fiber. Added features of this grade include: Electrically Conductive, Ultra High Modulus and Strength, Easy Molding, Excellent Wear Resistance and Low CTE.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Good dimensional stability,Wear resistant,Good Mold Release,Electrically Conductive,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Density 1.50 g/ccASTM D792
Moisture Absorption 0.0100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0020 - 0.0030 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 251 MPa5 mm/min; ASTM D638
 270 MPa5 mm/min; ISO 527
Elongation at Break 1.3 %5 mm/min; ASTM D638
 1.4 %5 mm/min; ISO 527
Tensile Modulus 44000 MPa5 mm/min; ASTM D638
 44000 MPa1 mm/min; ISO 527
Flexural Strength 383 MPa1.3 mm/min, 50 mm span; ASTM D790
 404 MPa2 mm/min; ISO 178
Flexural Modulus 37000 MPa1.3 mm/min, 50 mm span; ASTM D790
 39100 MPa2 mm/min; ISO 178
Izod Impact Notched 68.1 JASTM D256
Izod Impact, Unnotched 503 J/mASTM D4812
Izod Impact, Notched (ISO) 7.70 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 42.9 kJ/m²80*10*4; ISO 180/1U
Charpy Impact Unnotched 52.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.70 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmASTM D257
Surface Resistance 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 1.70 µm/m-°C
@Temperature -40.0 - 120 °C
ASTM E831
CTE, linear, Transverse to Flow 48.0 µm/m-°C
@Temperature -40.0 - 120 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 337 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 338 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 330 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 329 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 380 - 400 °C
Zone 2 360 - 370 °C
Zone 3 370 - 380 °C
Melt Temperature 380 - 400 °CInjection Molding
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Screw Speed 50 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81675 / 289622

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.