MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Teijin Films Melinex® 3380 & CORE 1 Polyester Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® 3380 and Melinex® CORE1 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and other polyesters, as well as a variety of substrates. The two films are identical except that CORE1 is supplied sheeted with the heat seal surface modified to prevent air entrapment during lamination. CORE1 is required where two layers of CORE1 are laminated to each other as part of the card construction. These two films are currently available at thicknesses of 600 gauge and 1210 gauge.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D1505
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 100 %100 %ASTM D882A
Film Elongation at Break, TD 80 %80 %ASTM D882A
Film Tensile Strength at Break, MD 68.9 MPa10000 psiASTM D882A
Film Tensile Strength at Break, TD 68.9 MPa10000 psiASTM D882A
Heat Seal Strength >= 1800 g/25 mm>= 3.97 lb/inDTF (US) Test Method No. 2.49
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 2.0 %
@Temperature 190 °C,
Time 300 sec
2.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.0 %
@Temperature 190 °C,
Time 300 sec
2.0 %
@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Optical Density  0.90
@Thickness 0.152 mm
0.90
@Thickness 0.00600 in
[%]; DTF (US) Test Method 2.30.2
 1.8
@Thickness 0.307 mm
1.8
@Thickness 0.0121 in
[%]; DTF (US) Test Method 2.30.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® 339 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® 339 Polyester Film, 1000 Gauge
DuPont Teijin Films Melinex® 3381 Polyester Film
DuPont Teijin Films Melinex® 331W Polyester Film, 200 Gauge

PDTZ9049 / 139446

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.