MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Morgan Advanced Ceramics GBC-92% Alumina 92-SV Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Highly versatile alumina ceramic with great mechanical, electrical, thermal, and chemical properties.

Prime Features:

  • Excellent electrical properties
  • High mechanical strength and wear resistance
  • Chemical and corrosion resistance
  • Consistent electrical and mechanical properties
  • Thermal stability
  • Dense, non porous and vacuum tight
Typical Applications:
  • Electrical packages
  • Lids and Covers
  • Bushings
  • Grinding media
  • Wear resistance components
  • General industrial duties requiring great mechanical, electrical, and thermal properties
Production Capabilities:
  • High volume production
  • Tight tolerance pressed alumina parts
  • Multi-cavity tooling
  • Complex geometries and multi-level configurations
  • Sub-miniature designs
  • Design consultation

Information provided by Morgan Advanced Materials

Key Words: 92-SV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.65 g/cc0.132 lb/in³
Open Porosity 0.00 %0.00 %fully dense, % nominal, apparent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Tensile Strength 193 MPa28000 psi
Flexural Strength 379 MPa55000 psi
Compressive Strength 1930 MPa280000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmat RT
Dielectric Constant 8.6
@Frequency 1e+6 Hz
8.6
@Frequency 1e+6 Hz
at RT
Dielectric Strength 8.27 kV/mm210 kV/in
Dissipation Factor 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.10 µm/m-°C3.94 µin/in-°F
Thermal Conductivity 19.0 W/m-K132 BTU-in/hr-ft²-°Fat RT
 
Component Elements PropertiesMetricEnglishComments
Al2O3 92 %92 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armstrong A-12 Epoxy Adhesive, at 2:3 Mix Ratio
92% Alumina, opaque
Morgan Advanced Ceramics GBC 92% Alumina
GBC Grade 92 Alumina
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150-M

CMORF5009 / 200247

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.