MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sasol Polymers PP HSV103 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: Features: High flow; Narrow molecular weight distribution; Offers easy extrusion processability when used for producing: Spunbonded non-woven materials; BCF carpet yarn on in-lin or two stage spin/draw/wind or short spin/warp draw/wind processes; Continuous filament (CF) on multi position spin/draw/wind processes. Applications: Extrusion: Spunbond fabric for industrial applications (roof membranes, geotextiles); Spunbond fabrics for hygiene applications (nappy liners, medical gowns and masks); Carpet yarns; Extrusion coating of woven PP cloth; Hair braids
Availability: Africa & Middle East; Asia Pacific, Europe, Latin America, North America
Additive: Anti-gas fading; Processing Stabilizer
Features: Gas-fading Resistant; Good processability; Good Processing Stability; High Flow; Homopolymer; Narrow Molecular Weight Distribution
Uses: BCF Yarn; Fabrics; Filaments; Industrial Applications; Spunbond Nonwovens; Wovens Coatings
Forms: Pellet
Processing Method: Extrusion

Information provided by Sasol Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psiISO 527-2/1A/50
Elongation at Break >= 50 %>= 50 %ISO 527-2/1A/50
Elongation at Yield 8.5 %8.5 %ISO 527-2/1A/50
Tensile Modulus 1.40 GPa203 ksiISO 527-2/1A/50
Flexural Modulus 1.35 GPa196 ksiISO 178
Charpy Impact, Notched 0.252 J/cm²1.20 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 325 °C617 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 82.8 °C181 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C126 °FUnannealed; ISO 75-2/A
Vicat Softening Point 87.8 °C190 °FISO 306/B120
 152 °C306 °FISO 306/A120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 60.0 °C104 - 140 °FHopper
Zone 1 200 - 280 °C392 - 536 °F
Zone 2 240 - 280 °C464 - 536 °F
Zone 3 240 - 280 °C464 - 536 °F
Zone 4 240 - 280 °C464 - 536 °F
Zone 5 220 - 280 °C428 - 536 °F
Die Temperature 220 - 240 °C428 - 464 °F
Melt Temperature 220 - 280 °C428 - 536 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSASOL006 / 268335

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.