Mumetal – Permimphy are the crystalline soft magnetic alloys with very high permeability, linear, stress resistant and the lowest magnetic losses. Applications: - Magnetic shielding
- Current sensors
- High precision current transformer cores
- Ground fault circuit breaker (relay parts)
Standards relative to these applications : ASTM A753Information provided by Aperam |