MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Crosspolimeri CROSSVINIL EK/2 AZOR UV PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Crossvinil: we have studied a special series of PVC compounds.

Crossvinil EK/2 AZOR UV: Standard for flame retardant and high temperature sheathing cable extrusion. The material is also UV and oil resistant.

Certify: CEI 2011 TM3,BS 7655 TM3, VDE 0207 YM4,IEC 60332-3, IEC 60502 ST1 80°C - ST2 90°C.

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength 14.0 MPa2030 psiIEC 60811
 >= 17.5 MPa
@Temperature 100 °C,
Time 605000 sec
>= 2540 psi
@Temperature 212 °F,
Time 168 hour
Heat Ageing; IEC 60811
 >= 18.2 MPa
@Temperature 100 °C,
Time 252000 sec
>= 2640 psi
@Temperature 212 °F,
Time 70.0 hour
Ageing in oil ASTM II
Elongation at Break 240 %240 %IEC 60811
 >= 300 %
@Temperature 100 °C,
Time 605000 sec
>= 300 %
@Temperature 212 °F,
Time 168 hour
Heat Ageing; IEC 60811
 >= 336 %
@Temperature 100 °C,
Time 252000 sec
>= 336 %
@Temperature 212 °F,
Time 70.0 hour
Ageing in oil ASTM II
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 35 %35 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Zone 1 140 °C284 °F
Zone 2 145 °C293 °F
Zone 3 155 °C311 °F
Zone 4 160 °C320 °F
Die Temperature 175 °C347 °F
Head Temperature 170 °C338 °F
 
Descriptive Properties
Cold Flex-15°CISO 458
Thermal stability100 min200°C, ISO R 182/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS007 / 294091

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.