MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4406 G4 Q113 20% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %23°C/50% R.H.; ISO 62
Viscosity Number 112 cm³/g
Linear Mold Shrinkage 0.0030 cm/cmASTM Data; MD
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 117 MPa0.2 in/min; ASTM Test
Tensile Strength, Ultimate 117 MPa5mm/min; ISO 527
Elongation at Break 2.2 %5mm/min; ISO 527
 2.2 %
Tensile Modulus 8280 MPaASTM Test
 8350 MPa1mm/min; ISO 527
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
ASTM Test
Charpy Impact Unnotched 3.60 J/cm²ISO 179
 5.00 J/cm²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 0.600 J/cm²ISO 179
 NB
@Temperature -30.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
 3.7
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0016
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
CTE, linear, Parallel to Flow 50.0 µm/m-°CISO 11359
Melting Point 223 °C10 K/min
 223 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 215 °CASTM Test
 215 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 177 °CASTM Test
 180 °CISO 75
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 265 °CInjection molding
Injection Velocity 70.0 mm/secInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicFlame retarding agent
 Heat stabilized or stable to heat
 Light stabilized or stable to light
 Lubricant
 U.V. stabilized or stable to weather

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4406 G6 Q113 30% Glass Filled PBT
BASF Ultradur® B 4520 PBT
BASF Ultradur® B 4406 G4 BKQ113 7110 20% Glass Filled PBT
BASF Ultradur® B 2550 PBT
Akro-Plastic Akromid® A3 GF 25 1 L black (4672) PA66 + PP, Dry, 25% Glass Filled

PBASF9083 / 84847

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.