MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistance

Information provided by Wanhua Chemical Group Co., Ltd.

Key Words: FDA 21 CFR 177.1680, 177.2600; USP VI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength 25.0 MPaASTM D412
Elongation at Break 600 %ASTM D412
100% Modulus 0.00600 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0100 GPa
@Strain 300 %
ASTM D412
Tear Strength 75.0 kN/mASTM D624
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -45.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Taiwan PU Corporation UR50 Polyester Urethane Rubber
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
Celanese Ateva® 2803G Ethylene Vinyl Acetate Copolymer
Westlake Plastics Pomalux® Acetal Copolymer, Compression Molded
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether

PWANTH953 / 156376

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.