MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applications such as consumer electronics, office equipment, building & construction, housewares, office products, cosmetics & personal care products, recreation equipment & sporting goods, toys, and furniture & furnishings.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Moisture Absorption at Equilibrium <= 0.10 %23°C/50% RH
Water Absorption at Saturation <= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 55ASTM D785
Tensile Strength at Break 17.0 MPaASTM D638
Tensile Strength, Yield 20.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 2.068 GPaASTM D638
Flexural Modulus 2.275 GPaASTM D790-1
Izod Impact, Notched 3.40 ft-lb/inASTM D256-A
Gardner Impact 320 in-lb
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D5420, GB
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °CASTM D648
Vicat Softening Point 97.0 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
all colors
 
Optical PropertiesOriginal ValueComments
Gloss 70 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 280 °CMolding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Dow AIM® 4810 High Impact Styrenic Resin
Dow AIM® 4800 High Impact Styrenic Resin
LG Chemical ALPHALAC SG910 HIPS
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)

PSG106 / 67267

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.