MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper nickel 10%, UNS C70600, OSO35 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Good hot and cold workability. Fabricated by forming and bending, welding.

Applications: condensers, condenser plates, distiller tubing, evaporator and heat exchanger tubing, ferrules, salt water piping.

Test specimen: flat products - 1mm thickness.

Key Words: CDA 706, CN102, ISO CuNi10Fe1Mn; 90-10 Cupronickel
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 2727
Hardness, Rockwell F 7373
Tensile Strength, Ultimate 358 MPa51900 psi
Tensile Strength, Yield  98.0 MPa
@Strain 0.2 %
14200 psi
@Strain 0.2 %
 98.0 MPa
@Strain 0.5 %
14200 psi
@Strain 0.5 %
Elongation at Break 35 %35 %in 50 mm
Modulus of Elasticity 140 GPa20300 ksi
Poissons Ratio 0.350.35Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 52.0 GPa7540 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000190 ohm-cm
@Temperature 20.0 °C
0.0000190 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
9.50 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 40.0 W/m-K278 BTU-in/hr-ft²-°F
 59.5 W/m-K
@Temperature 100 °C
413 BTU-in/hr-ft²-°F
@Temperature 212 °F
Mill Annealed
 70.2 W/m-K
@Temperature 200 °C
487 BTU-in/hr-ft²-°F
@Temperature 392 °F
Mill Annealed
 78.5 W/m-K
@Temperature 300 °C
545 BTU-in/hr-ft²-°F
@Temperature 572 °F
Mill Annealed
 82.8 W/m-K
@Temperature 700.0 °C
575 BTU-in/hr-ft²-°F
@Temperature 1292 °F
Mill Annealed
 84.0 W/m-K
@Temperature 400 °C
583 BTU-in/hr-ft²-°F
@Temperature 752 °F
Mill Annealed
 86.3 W/m-K
@Temperature 600.0 °C
599 BTU-in/hr-ft²-°F
@Temperature 1112 °F
Mill Annealed
 86.6 W/m-K
@Temperature 500 °C
601 BTU-in/hr-ft²-°F
@Temperature 932 °F
Mill Annealed
Melting Point 1100 - 1150 °C2010 - 2100 °F
Solidus 1100 °C2010 °F
Liquidus 1150 °C2100 °F
Annealing Point 593 - 816 °C1100 - 1500 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 600 - 825 °C1110 - 1520 °F
Hot-Working Temperature 850 - 950 °C1560 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88.7 %88.7 %
Iron, Fe 1.0 - 1.8 %1.0 - 1.8 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 9.0 - 11 %9.0 - 11 %
Other, total <= 0.50 %<= 0.50 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 10%, UNS C70600
Copper nickel 10%, UNS C70600, OSO50 Temper flat products
Copper nickel 10%, UNS C70600, H06 Temper flat products
Copper nickel 10%, UNS C70600, H04 Temper flat products
Copper nickel 10%, UNS C70600, H02 Temper flat products

MC70600b3 / 11719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.