MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Alfa Chemistry Materials Cerium Chloride Anhydrous
Categories: Ceramic; Halide

Material Notes: Cerium Chloride, in forms of crystalline aggregates or light yellow lump aggregates, is the important material for catalyst, glass, phosphors and polishing powders. It is also used to decolorize glass by keeping iron in its ferrous state. The ability of Cerium-doped glass to block out ultra violet light is utilized in the manufacturing of medical glassware and aerospace windows. It is also used to prevent polymers from darkening in sunlight and to suppress discoloration of television glass. It is applied to optical components to improve performance.

Applications: Used as petroleum catalyst, automobile exhaust catalysts, organic synthesis catalyst, pharmaceutical intermediates, also used as a starting point for the preparation of other cerium salts, such as the Lewis acid, cerium(III) trifluoromethanesulfonate, used for Friedel-Crafts acylations. It can be used itself as a Lewis acid, for example as a catalyst in Friedel-Crafts alkylation reactions.

Solubility: Soluble in water, Insoluble in Pyridine material.

Molecular Formula: CeCl3

Room temperature, sealedAlfa Chemistry Materials product group: Metal

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.92 g/cc
Molecular Weight 246 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 848 °C
Boiling Point 1727 °C
 
Descriptive Properties
AppearanceWhite crystalline
CAS Number779008-60-5
Purity99.999% 99.99% 99.9% 99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ZZALFA66420 / 303158

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.