MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
MOL Group TATREN IM 45 54 PP, Impact copolymer for injection molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: TATREN IM 45 54 is a high crystallinity impact copolymer of good processing stability and medium fluidity. This grade shows excellent organoleptic properties of the typical MOL in-reactor made grades. The improved polymer structure combined with the built-in additivation package gives potential for shorter cycle time and wall thickness reduction. This grade is additivated by nucleating and antistatic agent. TATREN IM 45 54 is characterized by very high stiffness with well balanced impact resistance.

Applications: TATREN IM 45 54 is intended especially for thin wall injection molding (TWIM) of products where high wall stiffness combined with good impact resistance is required – rigid food and non-food packages, hot-filled application, household articles, consumer goods etc. Another typical end products are buckets for paints and coatings, storage and transport containers, crates, garden furniture, flower pots, toys and different technical items. This grade is particularly suitable also for automotive applications.

(1) Typical properties measured on standard injection molded test specimen according to ISO 294-1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 45 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
Storage Temperature <= 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 971; ISO 2039-2
Tensile Strength, Yield 29.5 MPa1; ISO 527-1,2
Elongation at Yield 4.5 %1; ISO 527-1,2
Modulus of Elasticity 1.80 GPa1, in Tension; ISO 527-1,2
Flexural Modulus 1750 MPa1; ISO 178
Izod Impact, Notched (ISO) 3.30 kJ/m²
@Temperature -20.0 °C
1; ISO 180/A
 5.50 kJ/m²
@Temperature 23.0 °C
1; ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C1, flatwise; ISO 75-1,2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOLG101 / 297267

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.