MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Traid Villarroya TVH® TV25 (GG25) Perlitic Cast Iron with Lamellar Graphite, Continuous Cast
Categories: Metal; Ferrous Metal; Cast Iron

Material Notes:
  • Machinability: very good
  • Wear resistance: very good
  • Inductive or flame-hardening capacity: good
  • Nitride hardening capacity: good
  • Quenching: very good
  • Weldability: partially weldable with special electrodes
Industry Applications:
  • Compressors
  • Cylinders
  • Pistons
  • Pumps

Information provided by Traid Villarroya Hnos. S.L.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.15 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 250 - 350 MPaRm
Tensile Strength, Yield 165 - 228 MPaRp 0.2
Elongation at Break 0.80 %A
Modulus of Elasticity 103 - 118 GPa
Flexural Strength 340 MPaddß
Compressive Strength 840 MPaddß
Poissons Ratio 0.26
Shear Strength 290 MPaddß
 290 MPaTorsional, ddß
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 47.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 2.9 - 3.1 %
Iron, Fe 93.7 - 94.5 %As Remainder
Manganese, Mn 0.80 - 1.1 %
Silicon, Si 1.8 - 2.1 %
 
Descriptive Properties
Alternating tensile-comp. strength60 MPa
Fracture toughness KIC480 N/mm3/2
Reversed bending strength120 MPadbß

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NTRAID952 / 318919

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.