MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.

Electro 170 is a specialty grade, peroxide curable silicone elastomer.

Key Feature: Excellent Tracking and erosion resistance (1a 4.5KV); improved hydrophobicity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.57 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
Tensile Strength 5.50 MPa
Elongation at Break 250 %
Tear Strength 16.0 kN/mDie B
 
Descriptive Properties
AppearanceGrey

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive
Momentive Performance Materials Silopren™ LSR 2660 ZKS Custom Liquid Silicone Rubber - Automotive
CHT Group QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material
Rogers Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate
NuSil MED-4801 Liquid Silicone Rubber - Unrestricted Medical Use

PGE8V868 / 109128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.