MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dezincification Brass, DZR, UNS C35330
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Dezincification resistant brass suitable for high speed machining applications

Applications: The alloy is best suitable where potential corrosion (such as dezincification) may occur. Applications for this alloy include plumber's hardware, valve spindles and fittings.

Information Provided by Mueller Industries Inc.

Key Words: AS 1567, UNS C35330, BS 2873 - C2119
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 60
Tensile Strength at Break 54000 psi
Tensile Strength, Yield 24000 psi
Elongation at Break 30 %
Tensile Modulus 15000 ksi
Machinability 100 %UNS C36000 = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm26% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µin/in-°F
@Temperature 20.0 - 300 °C
Melting Point 1645 - 1660 °F
Solidus 1645 °F
Liquidus 1660 °F
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As 0.020 - 0.25 %
Copper, Cu 59.5 - 64 %
Lead, Pb 1.5 - 3.5 %
Zinc, Zn 32.25 - 39 %Remainder

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-cutting phosphor bronze, UNS C54400, H04 Temper 25 mm rod
Low-silicon bronze B, UNS C65100, H04 (36%) Temper rod
316 Stainless Steel, annealed and cold drawn bar
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO35 Temper rod
Forging Brass, UNS C37700

MC35330b1 / 160289

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.