MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Embrace™ LV Renew-35 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: The world's leading shrink film just got better with the introduction of Eastman Embrace™ LV Renew-35 copolyester to the Eastman Embrace™ family of resins. LV stands for LOW shrink force and VERSATILE shrink curve. Living up to its name, it demonstrates its versatility with its ability to be produced with 40 to 50% reduction in shrink force, compared with other polyester shrink films and with a shrink curve that is similar to both PVC and OPS while still maintaining ultimate shrinkage greater than 75%. This versatility is achieved by making changes to the extruders manufacturing process. Eastman Embrace™ LV Renew-35 copolyester emulates all visually satisfying attributes expected from the current Eastman Embrace™ such as high gloss and clarity. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®. The GREENGUARD INDOOR AIR QUALITY CERTIFIED® Mark is a registered certification mark used under license through the GREENGUARD Environmental Institute (GEI). GEI is an industry-independent, non-profit organization that oversees the GREENGUARD Certification Program. The GREENGUARD Certification Program is an industry independent, third-party testing program for low-emitting products and materials for indoor environments. For more information about GEI and to obtain printable certificates for Eastman™ Copolyesters, visit www.greenguard.org . Choose Eastman Chemical Company under the Manufacturer category and click search to display a list of our products. This product has received a Platinum level Material Health Certificate from the Cradle to Cradle Products Innovation Institute. A Material Health Certificate is awarded to products that meet the Material Health requirements of the multi-attribute Cradle to Cradle Certified™ Product Standard. The Cradle to Cradle Products Innovation Institute is a nonprofit organization that administers the publicly available Cradle to Cradle Certified™ Product Standard, which provides designers and manufacturers with criteria and requirements for continually improving product materials and manufacturing processes. The Material Health Certificate provides manufacturers with a trusted way to communicate their efforts to identify and replace chemicals of concern in their products. For more information about Cradle to Cradle certification and to obtain printable certificates for Eastman copolyesters, visit www.c2ccertified.org . Search for Eastman Chemical Company in the Material Health Certificate Registry. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Decorative laminates-cabinetry
  • Decorative laminates-wood
  • Home, garden & automotive packaging
  • Labels non food contact
  • Multi-layer film non food contact
  • Shrink film food contact
  • Shrink film non food contact
Key Attributes
  • Customizable shrink curve
  • Eye-catching 360° graphic capability
  • Greater than 75% ultimate shrinkage
  • Low shrink force
  • Optimal machine direction growth
  • Shrinks to fit contour bottles
  • Sparkling clarity and high gloss
  • Super-high print definition

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Extruded/Cast Film; ASTM D1505
 1.30 g/cc0.0470 lb/in³Stretched Film; ASTM D1505
Water Vapor Transmission 6.70 g/m²/day0.431 g/100 in²/dayExtruded/Cast Film; ASTM F1249
 25.0 g/m²/day1.61 g/100 in²/dayStretched Film; ASTM F1249
Oxygen Transmission 3.90 cc-mm/m²-24hr-atm9.91 cc-mil/100 in²-24hr-atmStretched Film; ASTM D3985
 6.70 cc-mm/m²-24hr-atm17.0 cc-mil/100 in²-24hr-atmExtruded/Cast Film; ASTM D3985
Viscosity Measurement 0.7000.700Inherent, film (Extruded/Cast Film), EMN-A-AC-G-V-1
 0.7000.700Inherent, film (Stretched Film), EMN-A-AC-G-V-1
Thickness 50.0 microns1.97 milStretched Film
 250 microns9.84 milExtruded/Cast Film
Surface Tension 3.00 dynes/cm3.00 dynes/cmHarmonic Mean, Polar, Stretched Film
 44.0 dynes/cm44.0 dynes/cmHarmonic Mean, Dispersive, Stretched Film
 48.0 dynes/cm48.0 dynes/cmHarmonic Mean, Total, Stretched Film
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 43.0 MPa6240 psiStretched Film; ASTM D882
Film Tensile Strength at Yield, TD 105 MPa15200 psiStretched Film; ASTM D882
Film Elongation at Break, MD 4.00 %4.00 %Extruded/Cast Film; ASTM D882
 480 %480 %Stretched Film; ASTM D882
Film Elongation at Break, TD 4.00 %4.00 %Extruded/Cast Film; ASTM D882
 42.0 %42.0 %Stretched Film; ASTM D882
Film Elongation at Yield, MD 3.00 %3.00 %Stretched Film; ASTM D882
Film Elongation at Yield, TD 4.00 %4.00 %Stretched Film; ASTM D882
Tensile Modulus 1.90 GPa276 ksiMD, Extruded/Cast Film; ASTM D882
 1.90 GPa276 ksiTD, Extruded/Cast Film; ASTM D882
 2.00 GPa290 ksiMD, Stretched Film; ASTM D882
 5.30 GPa769 ksiTD, Stretched Film; ASTM D882
Tear Strength, Total 47.0 N10.6 lb (f)MD, PPT, Extruded/Cast Film; ASTM D2582
 62.0 N13.9 lb (f)TD, PPT, Extruded/Cast Film; ASTM D2582
Tear Strength 3.00 kN/m17.1 pliTD, Stretched Film, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min); ASTM D1938
 28.0 kN/m160 pliMD, Stretched Film, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min); ASTM D1938
 34.0 kN/m194 pliMD, Extruded/Cast Film, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min); ASTM D1938
 37.0 kN/m211 pliTD, Extruded/Cast Film, Tear Propagation Resistance, Split Tear Method @ 254 mm/min (10 in./min); ASTM D1938
Elmendorf Tear Strength MD 242 g242 gStretched Film; ASTM D1922
 704 g704 gExtruded/Cast Film; ASTM D1922
Elmendorf Tear Strength TD 864 g864 gExtruded/Cast Film; ASTM D1922
Film Tensile Strength at Break, MD 49.0 MPa7110 psiStretched Film; ASTM D882
 51.0 MPa7400 psiExtruded/Cast Film; ASTM D882
Film Tensile Strength at Break, TD 50.0 MPa7250 psiExtruded/Cast Film; ASTM D882
 258 MPa37400 psiStretched Film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 69.0 °C156 °FExtruded/Cast Film; ASTM D1525
Glass Transition Temp, Tg 69.0 °C156 °FExtruded/Cast Film; ASTM D1525
 69.0 °C156 °FStretched Film; ASTM D1525
Shrinkage >= 78.0 %
@Temperature 90.0 °C
>= 78.0 %
@Temperature 194 °F
Ultimate, Stretched Film
 
Optical PropertiesMetricEnglishComments
Haze 1.40 %1.40 %Extruded/Cast Film; ASTM D1003
 3.80 %3.80 %Stretched Film; ASTM D1003
Gloss 110 %110 %60°, Stretched Film; ASTM D2457
 161 %161 %60°, Extruded/Cast Film; ASTM D2457
Transmission, Visible 87.0 %87.0 %Regular, Stretched Film; ASTM D1003
 89.0 %89.0 %Regular, Extruded/Cast Film; ASTM D1003
 92.0 %92.0 %Total, Extruded/Cast Film; ASTM D1003
 92.0 %92.0 %Total, Stretched Film; ASTM D1003
 98.0 %98.0 %Transparency, Stretched Film; ASTM D1003
 99.0 %99.0 %Transparency, Extruded/Cast Film; ASTM D1003
 
Descriptive Properties
Color0.02a*, Stretched Film, ASTM D2244
 0.38b*, Stretched Film, ASTM D2244
 95.8L*, Stretched Film, ASTM D2244

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4138 / 323761

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.