MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NAECO® ELKON® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Precious Metal; Silver Alloy; Tungsten Alloy

Material Notes: For arcing and current carrying electrical contacts resistant to welding and sticking.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.27 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 91
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000367 ohm-cm(47% IACS)
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 175 W/m-K
Melting Point >= 980 °C
Solidus 980 °C
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 50 %
WC 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAECO® ELKON® G14 Tungsten Carbide Silver contact material ASTM 663, Class A, infiltrated
NAECO® ELKON® TC10 Tungsten Carbide Copper material
NAECO® ELKON® TC5 Tungsten Carbide Copper material
NAECO® ELKON® 3042 Silver Tungsten Carbide contact material ASTM B663
NAECO® ELKON® TC20 Tungsten Carbide Copper material

NCMV850 / 192421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.