MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik C0F Binderless Cemented Carbide, Seal Grade  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: Sandvik binderless carbide C0F exhibits excellent resistance to corrosion.

In applications where cemented carbide is in contact with corrosive media, particularly aqueous media, the metallic binder is slowly corroded, resulting in progressive wear of the cemented carbide. Corrosion cannot be completely avoided in cemented carbide with “corrosion resistant binders”. Without any binder, binderless is more resistant to corrosion than any other cemented carbide grade.

Features:

  • Binderless cemented carbide grade.
  • Very high hardness and excellent wear resistance due to the composition and the fine grain size.
  • Relatively low toughness, but higher toughness than ceramics (Al2O3, SiC, SiAlON).
  • Very high resistance to corrosion due to the absence of binder.
  • High thermal conductivity.
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 14.6 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell A 93.8
    Hardness, Vickers 190030
    Flexural Strength 1000 MPaTransverse Rupture; ISO 3327
     
    Descriptive Properties
    Corrosion Resistance, 1-109
    Wear Resistance, 0-109

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    China Tungsten YG6A Tungsten Carbide for Cutting Tools
    Sandvik H10F Extra-fine Grain Cemented Carbide for Rotary Tools
    Sapco Si.SiC Silicon Carbide
    China Tungsten YT30 Tungsten Carbide for Cutting Tools
    China Tungsten YG8 Tungsten Carbide for Cutting Tools

    NSANDV011 / 18905

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.