MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Heat-Away™ 641-EV Thermally Conductive Grease, Silver Filled, for High Vacuum Systems
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Aremco's Heat-Away™ thermal greases are ceramic and metal-filled silicone systems which offer exceptional thermal and electrical properties to 550 ºF. These materials are used in high-power electronic devices, heat pipes, and other heat exchange systems. Heat-Away™ 641-EV is an electrically and thermally conductive grease that is rated for high vacuum systems.

Aremco Heat-Away™ 641-EV Thermally Conductive Greases, Silver Filled, for High Vacuum Systems

Vendors: Aremco's Heat-Away™ greases are ceramic and metalfilled systems that offer exceptional electrical and thermal properties. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.30 g/cc
Solids Content 100 %
Water Absorption 0.00 %
Vapor Pressure 3.00e-14 torr
@Temperature 20.0 °C
 2.00e-12 torr
@Temperature 50.0 °C
 1.00e-9 torr
@Temperature 100 °C
 0.00000200 torr
@Temperature 200 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00020 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 5.58 W/m-K
Maximum Service Temperature, Air 550 °F
Minimum Service Temperature, Air -60.0 °F
 
Descriptive Properties
Chemical ResistanceExcellent
ColorSilver
FillerSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Sandvik Osprey CE7 Al-Si Controlled Expansion Alloy
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Fused Quartz
Borosilicate Glass, Low Expansion

CAREM993 / 138450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.